BESKRIVELSE Very hard and scratch resistant topcoat for painting of high quality furniture, doors and other wooden and fibre board surfaces indoors. Colours according to Temaspeed Premium tinting system. Aliphatic hardener 007 1250 is recommended for TAL-base due to its non-yellowing nature. Depending on the drying conditions hardener 0071250 might increase the paint gloss level.
PRODUKTEGENSKABER

 

ANBEFALEDE ANVENDELSER -

TEKNISKE DATA
Egenskaber Thinner 1069 (normal) or Thinner 1068 (slow).
Farve Område Colours according to TemaspeedPremium tinting system.
Glans grupper Mat
Dækning

8-10 m2/l (100 μm).       

Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Blandingsforhold Paint 100 parts by volume 588 -s
Harnder 50 parts by volume 007 1250 (aliphatic hardener)

Paint 100 parts by volume 588-s
Hardener 50 parts by volume 007 1378 (aromatic hardener)
Påførings metode

Application (+ 23 ºC)

 

Air assisted airless application with the viscosity 15-25 s (DIN 4) can be reached with approximately 10-20 % of thinning. Nozzle tip 0.011" - 0.015" and the nozzle pressure 100 - 180 bar. Atomising air pressure should be about 1 - 3 bar. Spray angle shall be chosen according to the shape of the object.

 

Conventional application with the viscosity 15 - 25 s (DIN 4) can be reached with approximately 10-20 % thinning. Nozzle tip 1.4 - 1.8 mm and the nozzle pressure 2 - 3 bar.

Pot-life (+23°C) 6 hours (0071378)
3 hours (0071250).
Tørretid

Drying times (100 - 120 g/m2)

 

Dust dry after 15 minutes in the room temperature 23 ºC.

Dry to stack minimum 8-24 hours in room temperature 23 ºC.

 

Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation. Stacking temperature of the painted objects below 35 ºC..
Tørstof volumen 57 weight-%, mixture 53 weight-%, (TAL-base)
58 weight-%, mixture 51 weight-%, (TCL-base)
Densitet 1,3 kg/litre.
Produktkode 588-s

PÅFØRING
Påførings-betingelser The surface to be painted has to be clean and dry. During application and drying the temperature of the air, the surface to be treated and the paint has to be at least 18 ºC and the relative humidity of the air below 70 %.
Forberedelse Primed surfaces must be sanded with roughness P320-400. All sanding dust must be removed with f.ex. air exhauster.
Grunding Novipur Primer HS.
Blanding af komponenter Stir the paint carefully before use. Add 50 volume-5 of hardener. thin the paint to the viscosity required.
Rengøring af værktøj Thinner 1069, 1082, 1068 or 1062.
EU VOC 2004/42/EC-limit værdi Maximum VOC content in ready to use mixture (thinned 10 % by volume) is 620 g/l.
For industrial use only.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
ProduktsikkerhedsdatabladNOVIPUR 30 [DK]
FortyndersikkerhedsdatabladTHINNER 006 1069 [DK]
HærdersikkerhedsdatabladHÆRDER 007.1250.
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.

Tilbage