Tikkurila worldwide
Tikkurila PRODUCT DATA SHEET
15.01.2010

Novipur 100

BESKRIVELSE -
PRODUKTEGENSKABER

Very hard and scratch resistant topcoat for painting of high quality furniture, doors and other wooden surfaces indoors.

Colour according to Temaspeed Premium tinting system.

Aliphatic hardener 007 1250 is recommended for TAL-base due to its non-yellowing nature.

ANBEFALEDE ANVENDELSER Novipur Primer HS can be used as primer before topcoat.

TEKNISKE DATA
Egenskaber Thinner 1068 and 1062 (slow thinner).
Farve Område Colours according to Temaspeed Premiun tinting system.
Glans grupper Helblank
Dækning

8-10 m2/l (100 μm).       

Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Blandingsforhold Paint - 100 parts by volume 587-s
Hardener - 50 parts by volume 007 1250 (aliphatic hardener)

or

Paint 100 parts by volume 587-s
Hardener 50 part by volume 007 1374 (aromatic hardener)
Påførings metode

Application (23 ºC)


 Air assisted airless application with the viscosity 15-22 s (DIN 4) can be reached with approximately 10-20 % of thinning. Nozzle tip 0.011" - 0.015" and the nozzle pressure 100 - 180 bar. Atomising air pressure should be about 1 - 3 bar. Spray angle shall be chosen according to the shape of the object.

 

Conventional application with the viscosity 15 - 22 s (DIN 4) can be reached with approximately 10-20 % thinning. Nozzle tip 1.4 - 1.8 mm and the nozzle pressure 2 - 3 bar.

Pot-life (+23°C) 8 hours.
Tørretid

Dust dry after 15 minutes in the room temperature 23 ºC .

Dry to stack minimum 24 hours in the room temperature 23 ºC .

 

Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation. Stacking temperature of the painted objects below  35 ºC .

Tørstof volumen 61 weight-%, mixture 55 weight-% (TAL-base)
62 weight-%, mixture 55 weight-% (TCL-base)
Densitet 1,2 kg/litre
Produktkode 587-s

PÅFØRING
Påførings-betingelser The surface to be painted has to be clean and dry. During application and drying the temperature of the air, the surface to be treated and the paint has to be at least 18 ºC and the relative humidity of the air below 70 %.
Forberedelse Primed surfaces must be sanded with roughness P600- 1000. All sanding dust must be removed with f.ex. air exhauster. Highest gloss level can be achieved by applicating two layers of Novipur 100 and sanding P1000 - 2000 between the layers.
Grunding Novipur Primer HS
Male Stir the paint carefully. Add 50 % by volume Hardener 007 1274 and mix well.
Thin the paint to the viscosity needed with Thinner 1068 or 1062. Proper spraying viscosity is 15-22 sec (Din4). The right nozzle size is 0,011-0,013” and angle 20 or 40 and the spraying distance from object about 20-25 cm.
Blanding af komponenter Stir the paint carefuly before use. Add 50 volume-% of hardener. Thin the paint to the viscosity required.
Rengøring af værktøj Thinner 1068, 1062, 1069 or 1082.
EU VOC 2004/42/EC-limit værdi Maximum VOC content in ready to use mixture (thinned 10 % by volume) is 620 g/l.
For industrial use only.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
ProduktsikkerhedsdatabladNOVIPUR 100 [DK]
FortyndersikkerhedsdatabladTHINNER 1061 [DK]
HærdersikkerhedsdatabladHÆRDER 007.1250.
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.

Tilbage