Tikkurila worldwide
Tikkurila PRODUCT DATA SHEET
07.09.2010

Temathane PC 80

BESKRIVELSE A high-solids two component, glossy polyurethane paint, hardener aliphatic isocyanate.
PRODUKTEGENSKABER Recommended as a glossy topcoat for epoxy systems exposed to weathering.
ANBEFALEDE ANVENDELSER Recommended for painting of storage tank exterios, steel buildings and other steelwork.

TEKNISKE DATA
Egenskaber Excellent weathering and abrasion resistance. A durable, easy to clean and non-chalking topcoat with good gloss and colour retention.
Farve kort RAL, NCS, SSG, BS, MONICOLOR NOVA and SYMPHONY colour cards. TEMASPEED tinting.
Glans grupper Blank
Dækning

Recommended film thicknesses

Theoretical coverage

dry

wet

 

80 µm

120 µm

8.3 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Fortynder 1048, 1067 og 1061
Blandingsforhold Base 5 parts by volume 524-series
Hardener 1 part by volume 008 7690 or 008 7590
Påførings metode By airless or conventional spray.
Pot-life (+23°C) 1½ hours
Tørretid

DFT 80 µm

+ 5 ºC

+ 10 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

2 h

1 h 15 min

1 h

20 min

Touch dry, after

10 h

8 h

6 h

3½ h

Recoatable, after

No limitations.


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Tørstof volumen 66 ± 2 % volume (ISO 3233)
77 ± 2 % weight
Densitet 1.3 ± 0.1 kg / l (mixed)
Produktkode 524-series

PÅFØRING
Påførings-betingelser All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below + 5 ºC during application or drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
Forberedelse Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Grunding Temacoat GPL-S Primer, Temacoat GF Primer, Temacoat HB Primer, Tembond, Temacoat RM 40, Temacoat SPA, Temadur 20, Temadur Primer, Temaprime GF, Fontecoat EP Primer and Fontecryl 10.
Toplak Temathane and Temadur.
Male By airless or conventional spray. In order to obtain an even, non-porous finish, spray a misty coat: first a thin layer, then let the solvents evaporate for 5 - 30 minutes and then apply the full coat. Depending on the application method and the termperature of the components (base, hardener, thinner) the paint can be thinned 0 - 15 %. Airless spray nozzle tip 0.011" - 0.013" and nozzle pressure 120 - 160 bar. Spray angle shall be chosen according to the shape of the object.
Overfladebehandling First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Blanding af komponenter Thinner 1048, 1067 or 1061.
EU VOC 2004/42/EC-limit værdi The Volatile Organic Compounds amount is 320 g/litre of paint mixture
VOC content of the paint mixture (thinned 15 % by volume) is 400 g/l.
For industrial and professional use only.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj.
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.

Tilbage