Tikkurila worldwide
Tikkurila PRODUCT DATA SHEET
03.01.2006

Temaprime EUR

BESKRIVELSE A fast drying, one component anti-corrosive alkyd primer.
PRODUKTEGENSKABER Primer in alkyd systems for steel surfaces exposed to weathering. Ideal for use in assembling plants and painting stations with rapid production cycles. Can also be used without any topcoat for steel surfaces in dry indoor areas.
ANBEFALEDE ANVENDELSER Recommended for steel structures, agricultural, construction and other machinery.

TEKNISKE DATA
Farve Område Reddish brown (TVT 4000) and grey (TVT 4001). TEMASPEED tinting.
Glans grupper Mat
Dækning

Recommended film thicknesses

Theoretical coverage

dry

wet

 

40 µm

80 µm

12.7 m2/l

60 µm

120 µm

8.5 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Fortynder 1006 og 1053
Påførings metode By airless spray or by brush
Tørretid

DFT 50 µm

+ 10 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

40 min

20 min

10 min

Touch dry, after

1½ h

40 min

30 min

Recoatable, after

1½ h

40 min

30 min


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Tørstof volumen 51 ± 2 % volume (ISO 3233)
70 ± 2 % weight
Densitet 1.3 kg / l
Produktkode 186-series

PÅFØRING
Påførings-betingelser All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +5 ºC during application or drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
Forberedelse Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean at least to grade Sa2. Clean small damages by tool cleaning to St2. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Grunding TEMAPRIME EUR.
Toplak TEMALAC, FONTECRYL and FONTELAC.
Male By airless spray or by brush. Mix the paint thoroughly before use. The paint can be thinned 0 - 15 % at airless spray application. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object.
Rengøring af værktøj Thinner 1006.
EU VOC 2004/42/EC-limit værdi The Volatile Organic Compounds amount is 440 g/litre of paint.
Maximum VOC content in ready to use paint (thinned 15 % by volume) is 495 g/l.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
ProduktsikkerhedsdatabladTEMAPRIME EUR [DK]
FortyndersikkerhedsdatabladTHINNER 1006 [DK]
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.