PRODUCT DATA SHEET 27.10.2008 |
|||||||||||||||||||||||||
Temadur SC 80 |
||||||||||||||||||||||||||
| BESKRIVELSE | A two component gloss polyurethane paint, containing anticorrosive pigments, hardener aliphatic isocyanate. | |||||||||||||||||||||||||
| PRODUKTEGENSKABER | Recommended especially to be used as a single coat finish for agricultural and earth moving machinery and other machinery and equipment. Also suitable to be used as a topcoat in epoxy/polyurethane systems exposed to weathering and chemical stress | |||||||||||||||||||||||||
| ANBEFALEDE ANVENDELSER | Storage tank exteriors, steel framework and other steel structures. | |||||||||||||||||||||||||
| TEKNISKE DATA | ||||||||||||||||||||||||||
| Egenskaber | Excellent weathering and abrasion resistance. A durable, easy to clean and non-chalking topcoat with good gloss and colour retention. | |||||||||||||||||||||||||
| Farve kort | RAL, NCS, SSG, BS, MONICOLOR NOVA and SYMPHONY colour cards. TEMASPEED tinting. | |||||||||||||||||||||||||
| Glans grupper | Blank | |||||||||||||||||||||||||
| Dækning |
Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated. |
|||||||||||||||||||||||||
| Fortynder | 1048 og 1067 | |||||||||||||||||||||||||
| Blandingsforhold | Base 5 parts by volume 532 series
Hardener 1 part by volume 008 7640 |
|||||||||||||||||||||||||
| Påførings metode | By airless or conventional spray. |
|||||||||||||||||||||||||
| Pot-life (+23°C) | 3 hours | |||||||||||||||||||||||||
| Tørretid |
Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation. When oven drying is practised in temperatures + 50 ºC - +100 ºC, the evaporation time should be 5 - 30 minutes before ovening, depending on the wet film thickness and actual temperature. |
|||||||||||||||||||||||||
| Tørstof volumen | 65 ± 2 % volume (ISO 3233)
80 ± 2 % weight |
|||||||||||||||||||||||||
| Densitet | 1.4 ± 0.1 kg / l (mixed) | |||||||||||||||||||||||||
| Produktkode | 532 series | |||||||||||||||||||||||||
| PÅFØRING | ||||||||||||||||||||||||||
| Påførings-betingelser | All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below + 5 ºC during application or drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point. | |||||||||||||||||||||||||
| Forberedelse | Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)
Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion. Zinc surfaces: Sweep blast clean with mineral abrasives, e.g. quartz sand, to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with FONTECLEAN ZN detergent. Hot dip galvanized surfaces are recommended to be painted with a mist coat (paint thinned 25 - 30 %) before the actual priming. Aluminium surfaces: Sweep blast clean with non-metallic abrasives to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with FONTECLEAN AL detergent. Note! Painted zinc and aluminium surfaces are not recommended when they are exposed to continuous condensation. Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4) |
|||||||||||||||||||||||||
| Grunding | TEMADUR PRIMER, TEMADUR 20, TEMACOAT GPL-S PRIMER, TEMACOAT GF PRIMER, TEMACOAT HB PRIMER, TEMACOAT PM PRIMER, TEMACOAT GPL-S MIO, TEMACOAT RM 40, TEMACOAT SPA MIO, TEMABOND, TEMAPRIME GF, FONTECRYL 10, FONTECRYL AP and FONTECOAT EP PRIMER. | |||||||||||||||||||||||||
| Toplak | TEMADUR and TEMATHANE. | |||||||||||||||||||||||||
| Male | By airless or conventional spray. Airless spray: depending on the temperature of the components and shape of the object the paint can be thinned 0 - 15 %. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 160 - 200 bar. Spray angle shall be chosen according to the shape of the object. In order to reach thicker coats (over 100 µm) use always "wet-in-wet" technique. At conventional spray the paint should be thinned 15 - 18 % to a viscosity of
20 - 25 s/DIN4. |
|||||||||||||||||||||||||
| Blanding af komponenter | First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing. | |||||||||||||||||||||||||
| Rengøring af værktøj | Thinner 1067 or Thinner 1048. | |||||||||||||||||||||||||
| EU VOC 2004/42/EC-limit værdi | The Volatile Organic Compounds amount is 320 g/litre of paint.
VOC content in paint (thinned 18 % by volume) is 420 g/l. |
|||||||||||||||||||||||||
| SUNDHED OG SIKKERHED KLASSIFICERING | ||||||||||||||||||||||||||
| Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy. | ||||||||||||||||||||||||||
| Produktsikkerhedsdatablad | TEMADUR SC 80 [DK] | |||||||||||||||||||||||||
| Fortyndersikkerhedsdatablad | THINNER 1067 [DK] | |||||||||||||||||||||||||
| Hærdersikkerhedsdatablad | HARDENER 008 7640 [DK] | |||||||||||||||||||||||||
| - | ||||||||||||||||||||||||||
Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.