Tikkurila worldwide
Tikkurila PRODUCT DATA SHEET
11.09.2007

Temablast EV 110

BESKRIVELSE Two component, iron oxide pigmented epoxy shopprimer.
PRODUKTEGENSKABER Protects blast cleaned steel during storage, fabrication and construction. Does not cause any harm during welding, cutting and burning or other treating of the steel.
ANBEFALEDE ANVENDELSER Blast cleaned steel.

TEKNISKE DATA
Egenskaber The product is found to comply with: Det Norske Veritas´ Offshore Standards, Det Norske Veritas´ Rules for Classification of Ships and Det Norske Veritas´ Type Approval Programme 1-602.2, 1999, Shop Primers for Corrosion Protection of Steel Plates and Sections. The shop primer is approved for application on blast cleaned steel plates and sections. For industrial use only according to Directive 1999/13/EC.
Farve Område Red
Glans grupper Mat
Dækning

Recommended film thicknesses

Theoretical coverage

dry

wet

 

20 µm

75 µm

13.5 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Fortynder 1031
Blandingsforhold Base 2 parts by volume 008 7920
Hardener 1 part by volume 008 7929
Påførings metode By spray.
Pot-life (+23°C) 24 hours
Tørretid

DFT 20 µm

+ 10 ºC

+ 23 ºC

+ 35 ºC

Touch dry, after

6 min

3 - 5 min

1 min

Recoatable, after

36 h

24 h

12 h


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Tørstof volumen 27 ± 2 % volume (ISO 3233)
48 ± 2 % weight
Densitet 1.2 kg / l (mixed)
Produktkode 008 7920

PÅFØRING
Påførings-betingelser All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below + 10 ºC during application or drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
Forberedelse Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.
Toplak Any type of paint with the exception of zinc rich paints. When selecting finishing coat for the shop primed surface, take into account the stress for which the object will be exposed. (SFS 8145)
Male By spray. If necessary, the paint can be thinned 0 - 5 % to a viscosity of 16 - 18 s DIN 4/20 ºC. Airless spray nozzle tip 0.011" - 0.018" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object.
Blanding af komponenter First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Rengøring af værktøj Thinner 1031.
EU VOC 2004/42/EC-limit værdi The Volatile Organic Compounds amount is 610 g/litre of paint.
VOC content of the paint mixture (thinned 5 % by volume) is 625 g/l.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
ProduktsikkerhedsdatabladTEMABLAST EV 110 [DK]
FortyndersikkerhedsdatabladTHINNER 1031 [DK]
HærdersikkerhedsdatabladTEMABLAST EV 110 HÆRDER - 008 7929[DK]
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.

Tilbage