Tikkurila PRODUCT DATA SHEET
22.02.2006

Fontecoat EP Primer

Coatings
BESKRIVELSE A two component waterborne epoxy primer.
PRODUKTEGENSKABER Used as a primer for steel surfaces in epoxy and polyurethane paint systems. Can be used on ships for surfaces above water line. Can also be applied onto concrete substrate e.g. walls, plasterboard etc.
ANBEFALEDE ANVENDELSER Recommended as a primer for haulage equipment, cranes, steel masts, conveyors and other steelwork, machinery and equipment.

TEKNISKE DATA
Farve Område Red TVT 4000, grey TVT 4004 etc.
Glans grupper Halvblank
Dækning

Recommended film thicknesses

Theoretical coverage

dry

wet

 

50 µm

105 µm

9.4 m2/l

70 µm

150 µm

6.7 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Fortynder Vand
Blandingsforhold Base 1 part by volume 007 1001-5
Hardener 1 part by volume 007 1019
Påførings metode By airless spray or brush.
Pot-life (+23°C) 1½ h
Tørretid

DFT 60 µm

+ 15 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

4 h

2 h

1 h

Touch dry, after

8 h

4 h

2 h

Recoatable by itself, after

12 h

6 h

3 h

Recoatable by solvent borne paints, after

48 h

24 h

12 h


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Tørstof volumen 47 ± 2 volume % (ISO 3233)
60 ± 2 weight %
Densitet 1.3 kg / l (mixed)
Produktkode 007 1001-5

PÅFØRING
Påførings-betingelser All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +15 ºC during application and drying. Relative humidity should not exceed 70 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
Forberedelse Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Grunding FONTECOAT EP PRIMER and TEMACOAT GPL-S PRIMER.
Toplak FONTECOAT EP 50, FONTECOAT EP 80, FONTEDUR 90, TEMACOAT GPL, TEMACOAT GS 50, TEMADUR and TEMATHANE.
Male By airless spray or brush. If necessary, the paint can be thinned maximum 5 %. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 140 - 180 bar. Spray angle shall be chosen according to the shape of the object.
Blanding af komponenter First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Rengøring af værktøj Water or a mixture of water and Thinner 1029, 1:1. The equipment must be cleaned immediately after use before the paint dries.
EU VOC 2004/42/EC-limit værdi The Volatile Organic Compounds amount is 60 g/litre of paint.
VOC content of paint mixture (thinned by 10 % by volume) 57 g/l.

SUNDHED OG SIKKERHED KLASSIFICERING
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
 
-

Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.