PRODUCT DATA SHEET 05.01.2011 |
|
Temafloor P 300 |
|
|
| BESKRIVELSE | A two component, solvent free epoxy coating. | |
| PRODUKTEGENSKABER | For new and old concrete floors exposed to heavy mechanical and chemical stress. | |
| ANBEFALEDE ANVENDELSER | Concrete floors in industrial and storage facilities, repair shops; e.g. process or paper machine units and corridors. | |
| TEKNISKE DATA | ||
| Egenskaber | Good resistance to abrasion. Withstands water, oils, greases, chemicals and dilute solutions of non-oxidizing acids, alkali and salt solutions. Resists only temporary splashes of oxidizing acids and bleaching chemicals. A separate chemical resistance table available. Withstands + 70 ºC dry heat and + 60 ºC in immersion. Does not resist abrupt, great or repeated changes of temperature. Self-levelling. Temafloor Flex hardener makes the paint surface flexible and thus more resistant to moving or cracking of concrete. Fire classification: BFL-s1 according to EN 13501-1. | |
| Farve Område | Sunlight will affect on the shade and the gloss of the coating in the long run. | |
| Farve kort | TEMASPEED tinting. Shade of TEMASPEED tinted product may differ from shade of in-plant tinted product. | |
| Glans grupper | Helblank | |
| Dækning | Coverage on concrete floors is on the average: Film thickness 0.3 mm coverage approx. 3 m2/litre Film thickness 0.5 mm coverage approx. 2 m2/litre Practical coverage depends on the porosity and evenness of the substrate and on the application method. |
|
| Blandingsforhold | Base 4 parts by volume 167-serie
Hardener 1 part by volume 008 4514, or Paint 2 parts by volume 167-serie Flex hardener 1 part by volume 930 5002 |
|
| Påførings metode | Pour the coating mixture onto the floor and spread it with a serrated steel trowel or a trowel. Level with a roller. | |
| Pot-life (+23°C) | 20 - 30 minutes on substrate, approx. 15 minutes in the mixing container. | |
| Tørretid ved 23°C og 50% relativ luftfugttighed | Dust dry after 6 hours Light trucking after 16 hours Fully cured after 7 days
At lower temperature the curing process will last longer. With Temafloor Flex hardener the curing times are a little longer than with standard hardener. |
|
| Tørstof volumen | Approx. 100 volume % | |
| Densitet | 1.4 kg / litre (mixture) | |
| Produktkode | 167-serie | |
| PÅFØRING | ||
| Påførings-betingelser | The relative humidity of the concrete should not exceed 97 %. The temperature of the ambient air, surface or coating should not fall below + 15 ºC during application or drying. Relative humidity of air should not exceed 80 %. | |
| Forberedelse | New concrete: Remove laitance by power grinding, vacuum grit blasting or hydrochloric acid etching. Choose the method best suited for the premises. After grinding remove dust carefully with a vacuum cleaner. Hydrochloric acid etching is carried out with diluted hydrochloric acid (1 part concentrated hydrochloric acid, 4 parts water). Rinse with plenty of water. Dry the floor.
Old concrete: Remove all grease, oil, chemicals and other impurities by MAALIPESU detergent. Remove old peeling paint layer by grinding or vacuum grit blasting. Choose the method best suited for the premises. Clean out pot-holes removing all loose friable material. Open cracks with e.g. an abrasive tool. Remove loose material and dust. |
|
| Grunding | Prime using 30 - 50 % with Thinner 1029 (or 1031) thinned Temafloor 200 or 400 epoxy varnish. Pour the varnish mixture onto the floor and apply as much as is needed to impregnate the concrete surface. If necessary, repeat priming to get a non-porous surface. Subsequent treatment can be carried out after 2 hours using "wet-on-wet" technique. A porous priming coat will result in holes and air bubbles in the finished screed. | |
| Patching | Patch pot-holes and cracks with Colofill putty or a mixture of unthinned Temafloor 200 epoxy varnish or Temafloor P 300 epoxy coating and dry, clean sand. Mixing ratio e.g. 1 part by volume of epoxy mixture and 1 - 2 parts by volume of sand of grain size 0.1 - 0.6 mm. Grind the patched areas before overcoating. | |
| Diluting | Do not thin Temafloor P 300 epoxy coating. | |
| Belægning | Overcoating may be carried out not earlier than 6 hrs and not later than 24 hrs after priming and patching. If the primed surface is not overcoated within 24 hrs, it should be abraded. Pour the coating mixture onto the floor and spread it with a serrated steel trowel or a trowel. Level with a roller. Recommended film thickness is 0.3 - 0.5 mm. | |
| Blanding af komponenter | Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes) by using a low speed hand drill with a paddle. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application. | |
| Rengøring af værktøj | Thinner 1029 or 1031. | |
| EU VOC 2004/42/EC-limit værdi | VOC 2004/42/EC (cat A/j) 500 g/l (2010)
Temafloor P300: max. VOC < 500 g/l |
|
| SUNDHED OG SIKKERHED KLASSIFICERING | ||
| Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj. | ||
| Produktsikkerhedsdatablad | TEMAFLOOR P300 and 3000 [GB-ENG] | |
| Fortyndersikkerhedsdatablad | THINNER 1029 [DK] | |
| Hærdersikkerhedsdatablad | TEMAFLOOR 100-200-P300 HÆRDER - 008 4514 [DK] | |
| - | ||
Ovenstående oplysninger er baseret på laboratorieforsøg og praktisk erfaring, og er gældende på datoen hvor dette datablad er trykt. Kvaliteten af produktet sikres ved vores operative system, baseret på kravene i ISO 9001 og ISO 14001. Som producent kan vi ikke være ansvarlig for eventuelle skader forårsaget ved brug af produktet mod vore anvisninger eller ved brug til uegnede formål.